Kromex® technology enables the shaping of logos, badges, emblems and any of the signs that identify your product.
Tooling costs are lower, comparing to other chrome technologies, as, for example, injection molding.
Technical specifications
Standard finishing
AUTOMOTIVE TESTS
TEST | REF. METHOD | TEST CONDITIONS | RESULTS |
---|---|---|---|
Heat Resistance | MS-CG12 | 250 h. at 80°C | no gloss change no delamination |
Humidity Resistance | MS-CG12 | 250 h. at 40°C 100% R.H. | no gloss change no delamination |
Salt Spray resistance | ASTM B117-95 | 200 h 38° C 5% NaCl | no gloss change no delamination |
Thermal Cycles | TSM 7508G | 2 h@-30°, 0,5 h @100°, 5 cycles | no gloss change no delamination |
Acid resistance | MS-CG12 | Spot Test 0,5-10% conc. | no gloss change no delamination |
Xenon WOM | SAE j1960-89 (2000 h) | UV < 380 nm Irradiance 50 W/m² |
no color change minimal gloss change |
Weathrometer QUV-A | SAE J 2020 | 1600 hh (8hUV 70° – 4hcond.50°C) | no color change minimal gloss change |